leaching method and process for secondary sulfide copper ore

     

Gas filled infiltration heap leaching method and process for secondary sulfide copper ore:

The secondary sulfide copper ore infiltration heap leaching method involves first laying an anti-seepage layer between the bottom pad and the retaining wall of the yard, then laying a collection pipe and a gravel layer, and finally laying an inflation pipeline and building the ore heap. The copper is extracted by leaching. The present invention embeds inflation pipelines in the process of building high clay ore piles, and efficiently introduces air into the interior of the yard through the inflation pipelines, thereby ensuring sufficient air inside the ore heap. 

At the same time, through the infiltration leaching method, high clay ore is immersed in the leaching solution for a long time, allowing the leaching solution, air, and high clay ore to fully contact each other for a long time, thereby ensuring efficient ore leaching. This allows high clay secondary sulfide copper ore to be produced using heap leaching, improving the utilization efficiency of copper resources.

+8613303827570
Related Product
Related Video
Product Center
Related Cases
Contact Us
We'll get in touch with you right away to provide detailed product info and tech insights sincerely.